ACID ETCHED GLASS / FROSTED GLASS
Frosted glass or Non-Fingerprint Glass,has a uniformly smooth,silk surface.Acid Etched Glass is translucent and matte in apperance.Acid etched glass transmits levels of diffused light,whilst providing privacy from adjacent glass. It is produced by acid etched one face or double face of the clear glass,ultra clear,tinted glass...Frosted glass or Non-Fingerprint Glass,has a uniformly smooth,silk surface.Acid Etched Glass is translucent and matte in apperance.Acid etched glass transmits levels of diffused light,whilst providing privacy from adjacent glass. It is produced by acid etched one face or double face of the clear glass,ultra clear,tinted glass...
Thickness
|
3-19mm
|
|||
Max Size
|
2440*6000mm
|
|||
Colors
|
Clear, Ultra clear, French green, Dark green, Euro grey, Dark grey, Ford blue, Dark blue, Ocean blue, Euro bronze, Dark bronze, Golden, Pink, Yellow, etc.
|
|||
Glass Type
|
Tempered glass, Heat strengthened glass, Tempered glass with heat soak, Bent tempered glass
|
|||
Package
|
Worthy export wooden crate, with plastic paper between each glass, suitable for export
|
|||
Applications
|
windows and doors in architecture Decorations Skylights Escalators Table tops and furniture Green house Facades and curtain walls Refrigerator shelves
Railings
Shower enclosures
Swimming pools |
|||
Certificate
|
GB15763.2 EN12150.1 EN12600 ANSIZ97.1 AS/NZS2008
|
Q1: How to judge the quality of float glass?
A1: Flatness, transparency, colorless, impurities, bubbles, etc.
Q2: How to reduce the self-implosion?
A2: The high quality float method is used for hot dip treatment, edge treatment and proper stress intensity. Pay attention to avoid side collision of glass during installation.
Q3: Scope of use of toughened glass?
A3: Safety is not involved in some parts of the building, but it is necessary to install toughened glass to improve the compressive strength and explosion-proof capacity,not to endanger the person safety
Q4: When toughened glass is broken, is the grain smaller the better?
A4: No, the smaller the particle, the easier it is to explode.
Q5: Can toughened glass and semi-toughened glass be made into laminated glass?
A5: Can't. The national standard stipulates: the glass that stresses the difference cannot make laminated glass, because in use process, the pressure that two pieces of glass bears is different.
Q6: Whether the laminated glass can fire, can the sound insulation?
A6: No, the smaller the particle, the easier it is to explode.
Q7: How many uv low-e glass can reduce?
A7: It is not fireproof glass, but has certain fireproof ability, also can soundproof, laminated glass is inside whole sound wave frequency range, in control noise is very good.
Q8: Does the air in the insulating glass do not oxidize the membrane?
A8: No, because there is a molecular sieve in the insulating glass, and the molecular sieve always keeps the air dry, so the membrane is not oxidized.
Q9: How much ultraviolet radiation can low-e glass reduce?
A9: It can reduce uv by 14% compared to heat reflecting glass. That's a 25 percent reduction in uv radiation compared to white glass.