Product
|
Pattern glass/Figured glass
|
|||
Glass thickness
|
3mm,4mm,5mm,5.5mm,6mm,8mm,10mm,12mm etc
|
|||
Glass color
|
Bule,Bronze,Clear,Green,Grey etc
|
|||
Size
|
2000*1500mm,2134*1524mm, 2200*1900mm, 2440*1830mm, 2500*2000mm, 2520*1530mm, 2520*1860mm, 2520*1880mm, 2550*1880mm etc. The size
can be customized according to your request. |
|||
Application
|
1. Windows,doors,
2. Skylights and canopies, 3. Glass stairs,balustrades, 4. Automotive windshield, 5. Facades and curtain walls |
|||
Features
|
1.Rich and colorful pattern designs provide unique decorative results: or obscure and quiet, or sparkling and lively, or serious
and elegant, or bold and generous; 2.Stereoscopic effect patterned and never fade; 3.Each distinctive pattern offers a different level of obscuration,providing privacy without sacrificing natural light; 4.Can be cut, ground, drilled, tempered, laminated and other deep-processing glass products |
|||
Application
|
1.Furniture & show shelves. 2.Areas where visual screen is required, like bathrooms, doors and windows. 3.Decorative illuminations
etc. |
Q1: How to judge the quality of float glass?
A1: Flatness, transparency, colorless, impurities, bubbles, etc.
Q2: How to reduce the self-implosion?
A2: The high quality float method is used for hot dip treatment, edge treatment and proper stress intensity. Pay attention to avoid side collision of glass during installation.
Q3: Scope of use of toughened glass?
A3: Safety is not involved in some parts of the building, but it is necessary to install toughened glass to improve the compressive strength and explosion-proof capacity,not to endanger the person safety
Q4: When toughened glass is broken, is the grain smaller the better?
A4: No, the smaller the particle, the easier it is to explode.
Q5: Can toughened glass and semi-toughened glass be made into laminated glass?
A5: Can't. The national standard stipulates: the glass that stresses the difference cannot make laminated glass, because in use process, the pressure that two pieces of glass bears is different.
Q6: Whether the laminated glass can fire, can the sound insulation?
A6: No, the smaller the particle, the easier it is to explode.
Q7: How many uv low-e glass can reduce?
A7: It is not fireproof glass, but has certain fireproof ability, also can soundproof, laminated glass is inside whole sound wave frequency range, in control noise is very good.
Q8: Does the air in the insulating glass do not oxidize the membrane?
A8: No, because there is a molecular sieve in the insulating glass, and the molecular sieve always keeps the air dry, so the
membrane is not oxidized.
Q9: How much ultraviolet radiation can low-e glass reduce?
A9: It can reduce uv by 14% compared to heat reflecting glass. That's a 25 percent reduction in uv radiation compared to white glass.